ISO 15609-5-2011 pdf free.Specification and qualification of welding procedures for metallic materials – Welding procedure specification -Part 5: Resistance welding. This part of ISO 15609 specifies requirements for the content of welding procedure specifications forresistance spot, seam, butt and projection welding processes. It is necessary to establish the acceptability ofapplying the principles of this part of lSO 15609 to other resistance and related welding processes before anyqualification is undertaken. NOTE Details of IS0 15609(all parts — for titles, see Foreword) are given in ISO 15607:2003,Annex A. Variables listed in this part of lSO 15609 are those influencing either weld dimensions (quality), weld nuggetdimension, weld pattern positioning, mechanical properties or geometry of the welded joint. Normative references The following referenced documents are indispensable for the application of this document.For datedreferences,only the edition cited applies.For undated references, the latest edition of the referenceddocument (including any amendments) applies. ISO 669, Resistance welding —Resistance welding equipment —Mechanical and electrical requirements ISO 4063,Welding and allied processes —Nomenclature of processes and reference numbers ISO5183 (all parts), Resistance welding equipment —Electrode adaptors, male taper 1:10ISO 5184,Straight resistance spot welding electrodes ISO 5821,Resistance welding —Spot welding electrode capsISO 5827,Spot welding – Electrode back-ups and clamps ISO 8205-1, Water-cooled…